How it is actually made
1. Dig and weather the clay
Brick clay is not pure kaolin. It is a mix of clay minerals, sand, silt, and iron oxide, and the mix matters: too much clay and the brick shrinks and cracks, too much sand and it crumbles. Freshly dug clay is left to weather outdoors for weeks or months, so that rain and frost break down the structure and make it more workable. Sand or ash is often blended in to control shrinkage.
2. Shape the brick
There are three routes. Extrusion pushes a stiff clay column through a die and cuts it with wires, which is how most modern bricks are made. Soft-mud moulding presses wet clay into sanded moulds, producing a softer, more irregular brick. Dry-press compacts low-moisture clay under high pressure, giving sharp edges and tight tolerances.
3. Dry before firing
Green bricks contain 10 to 20 percent water, and water turns to steam at 100 °C. Heat them too fast and the steam cannot escape, so the brick spalls or explodes. Drying is therefore a slow, controlled stage, often in a tunnel dryer at 80 to 120 °C for a day or more. Skipping it is the most common way to ruin a batch.
4. Fire to vitrification
Firing runs from about 900 °C for common bricks to 1,100 °C or more for engineering grades. At those temperatures the clay minerals dehydroxylate and then partially melt, and the glassy phase binds the remaining particles. The result is hard, porous, and dimensionally stable. Cooling must also be gradual, or thermal shock cracks the brick.
Why bricks are red
Iron oxide. Clay containing iron, fired in an oxygen-rich kiln, oxidises to haematite, which is red. Reduce the oxygen at the end of firing — the way a clamp kiln does when it is sealed — and the iron converts to magnetite, giving dark blue-grey bricks. The same clay can produce red or blue depending only on airflow.
Why some bricks are yellow or buff
Less iron and more lime. Clays with low iron and a calcium content fire to cream, buff, or yellow because there is not enough iron to form red haematite. This is a property of the deposit, not a coating, which is why matching a yellow brick for a repair is harder than matching a red one.